Anti Oxidant Superalloy Tungsten Carbide Plate For 3D Curved Glass Molding Machine

Contact Now
Zhuzhou Zhenfang Yaguang Tungsten Molybdenum Co., LTD.
City:zhuzhou
Province/State:hunan
Country/Region:china
Contact Person:MsShirley Pan
Contact Now

Anti Oxidant Superalloy Tungsten Carbide Plate For 3D Curved Glass Molding Machine

Ask Latest Price
Brand Name :Zhenfang
Model Number :ZF0192
Certification :ISO9001:2015
Place of Origin :China
MOQ :10 pcs
Price :USD 45-58/kg
Payment Terms :L/C, D/A, D/P, T/T, Western Union, MoneyGram
Supply Ability :10000 kg/month
Delivery Time :7-15 days
Packaging Details :follow customer requirements
material :100% Virgin Tungsten Carbide
surface :blank or grinding
Chemical Composition :Co-WC
Advantage :High Wear Resistance
grade :K10 K20 K30 etc
usage :for Mobile Phone 3D Glass Screen
more
Contact Now

Add to Cart

Find Similar Videos
View Product Description

Anti-oxidant superalloy tungsten carbide plate for 3D curved glass molding machine

Tungsten carbide heating plate is used on 3D curved glass molding machine, generally 6pieces for one set. Our carbide plate for 3D glass molding machine have high temperature resistant(over 800℃), high thermal conductivity.

Product Description
Product Name
super hard alloy cemented tungsten carbide plate for 3D curved glass bending machine
Material
tungsten carbide+Cobalt+Ni+Al+Cr etc.
Function
application for processing 3D mobile phone and watch glass hot bending molding machine
Package
by wooden case

Grade Information

Grade ISO Range Cobalt%

Density

g/cm3

Hardness

HRA

YG8 K30 8 14.8 89.5
YG6 K20 6 14.95 90.5
YG6X K10 6 14.95 91.5
YL10.2 K30 10 14.5 91.8
YG15 K40 15 14 87.5

Product application

Application Are: 3D Hot bending Glass Molding Machine

Super hard alloy tungsten carbide plate, mainly application for 3D curved glass hot bending molding machine , is widely used to process and form 3D curved glass of mobile phone, watch and TV. Compared with conventional tungsten steel plate and cemented carbide series, super hard alloy composite carbide plate has higher hardness, better high temperature deformation resistance, higher thermal conductivity and thermal diffusion coefficient when used at 900 ℃ high temperature . More stable performance greatly improves the production efficiency.

  • Product Advantages:

1. Excellent tensile strength:500-600MPa at 900 ℃;
2. High thermal shock resistance:fast heating up and cooling down available;
3. Good processability: workable in any condition according to customers’ need;
4. Super high temperature corrosion resistance: long service life without coating;
5. Strong chemical stability:No chemical reaction with glass,graphite and nitrogen;

6. Energy saving,environmental protection,good appearance of products.

If have any more information, please feel free to contact with me.

Web:www.tungstencarbide-rods.com
Tel: 0086-731-28215800
Fax: 0086-731-28215800
Mobile: 0086-13823202651(wechat/whatsapp)

Email address:sharon@chinahardalloy.com

Anti Oxidant Superalloy Tungsten Carbide Plate For 3D Curved Glass Molding Machine

Inquiry Cart 0